A freezing treatment - may be used between the first and second tempers. Freezing treatments help to attain maximum hardenability and must always be followed by at least one temper.
NOTE: For optimum stress relieving, CPM S30V may be tempered at 1000-1025?F (540-550?C). Tempering in this range may result in a slight decrease in corrosion resistance. Size Change: +0.05 to +0.10% when fully martensitic. The presence of retained austenite may reduce the net growth.